Resistencias para Galvanizados y Baños Químicos

Immersion Heaters for Plating Tanks

We build immersion heaters for electroplating, chrome, nickel, pickling and other corrosive chemical baths, in titanium, quartz, PTFE or stainless steel, chosen for the exact solution you are heating.

  • 5 options Available materials
  • Acid baths Quartz
  • Acid silver plating PTFE / Teflon
  • HCl · HF · nitric Titanium
  • Direct manufacturer
  • ISO 9001:2015
  • Reply in under 2 h
Who builds these heaters

Built here, not resold

Omega Heaters de México has spent over 25 years building industrial electric heating elements, and its tank heaters for plating and chemical processes come out of its own plant in Guadalupe, Nuevo León, Mexico. Direct manufacturer: you quote with the people who build your part.

ISO 9001:2015 ISO 9001:2015Certified processes and raw materials
  • Direct manufacturer Our own plant in Guadalupe, Nuevo León, Mexico. We are not distributors.
  • Over 25 years Building industrial electric heating elements for industry across northern Mexico.
  • ISO 9001:2015 Certified processes and raw materials, audited, with a warranty against manufacturing defects.
  • Five materials, not one Titanium, quartz, PTFE, 304/316 stainless and Incoloy 800 come out of the same plant, so our recommendation never depends on what is in stock.
  • We pick the material Tell us your chemistry and your concentration and we tell you which one survives your bath. The wrong material costs you the heater in weeks.
  • With low-level protection So the element never fires dry, which is how most of them burn out.
  • Shipping anywhere in Mexico From the plant in Guadalupe, Nuevo León, with the lead time confirmed when we quote.
Technical data

Specifications

Titanium
The highest chemical resistance, strong acids included
Quartz
For acid baths, with the element visible for inspection
PTFE / Teflon
For acid silver plating, at moderate temperature
304/316 stainless steel
For neutral or mildly aggressive solutions
Incoloy 800
For water, salts and mild alkaline solutions
How it is chosen
Give us your chemistry and concentration and we specify it
Mounting
Horizontal or vertical on the tank wall
Protection
Low-level cutoff, so it never fires dry

Aplicaciones

  • Tanques de galvanoplastia: zincado, niquelado, cromado, cobreado, dorado, plateado.
  • Acid or alkaline pickling and degreasing baths.
  • Tanques de anodizado.
  • Electrolytic baths and surface treatment baths generally.
  • Quenching processes in salts or saline solutions.

Qué ganas

  • Long service life when the material is chosen correctly for your specific chemistry. The number one cause of early failure in this kind of heater is the wrong material, not a manufacturing defect.
  • It protects your process: an incompatible material can contaminate the bath with corrosion particles and spoil the quality of the finish.
  • Mounting options to suit your tank: horizontal where there is side access, vertical where the wall cannot be drilled.
  • Dry-fire protection, which prevents element failure from loss of liquid or a low level.
Elige la mejor opción

¿Qué material necesita tu baño?

No hay un material "universal" para químicos corrosivos — el material correcto depende de la solución exacta que vas a calentar. Dinos qué proceso corres y te recomendamos el material; mientras tanto, esta es la guía general.

Titanio

The most corrosion-resistant of the four materials. Ideal for hydrochloric, hydrofluoric, nitric and chromic acid. It is the recommended choice when the bath is chemically aggressive and you need the longest possible service life.

Cuarzo

It withstands solutions from pH 0 to 7, except hydrofluoric acid and caustic (alkaline) solutions. It costs less than titanium and PTFE, which makes it common in nickel and chrome plating tanks whose solution sits in that pH range. It is mechanically fragile and needs care in handling and installation.

PTFE / Teflón (fluoropolímero)

Recommended for most acid plating solutions and pickling tanks, and the preferred choice where hydrofluoric acid is present at low concentrations, under 9%, which quartz cannot take. It withstands operating temperatures up to 88 °C / 190 °F.

Acero inoxidable 304/316 e Incoloy

Enough for less aggressive solutions: water, mild alkaline solutions, some quenching or saline baths. It is the economical choice when your process does not demand extreme chemical resistance.
EMERGENCY SUPPORT

Tank heater perforated? Send a photo on WhatsApp.

Tell us what solution you are heating and at what concentration. With that an engineer will tell you right away the correct material — titanium, quartz, PTFE or stainless steel — so it does not perforate again or contaminate your bath, and how long it takes.
1

Tell us the chemical, or the name of the process

chrome plating, nickel plating, pickling or another, with the concentration if you have it.
2

Send the dimensions of your tank and the kind of access

from the side, from the top, with or without the option of drilling the wall.
3

We recommend the material and the mounting

horizontal or vertical, to suit your solution and your tank.

Te contesta un ingeniero de aplicaciones

Lun–Vie 9:00–17:00 · respuesta < 2 h
Frequently asked questions

What we get asked most

How do I know which material my bath needs?
It depends on the exact chemical, its concentration and the operating temperature — not just on the name of the process. Tell us which solution you run (or the process name: chrome, nickel or zinc plating, and so on) and we will confirm the right material before building. If you are unsure, your chemical supplier can confirm it too.
Why did my last heater fail so fast?
The most common cause in this kind of application is a sheath material that is incompatible with the bath's actual chemistry — not a manufacturing defect. If your last heater was stainless steel and your solution is a strong acid, that was most likely the problem.
Can I use quartz in any acid bath?
Not in all of them: quartz holds up well in most solutions from pH 0 to 7, but it is not compatible with hydrofluoric acid or with caustic solutions. For those, PTFE or titanium are the right choices.
Which mounting do I need, horizontal or vertical?
If your tank allows a side penetration, horizontal mounting — through the wall, with a threaded fitting or a flange — is the most common. If you cannot drill the wall, vertical mounting with an IP67 head, which never touches the fluid, is the alternative.
What is the lead time?
4 to 6 business days in standard materials. Quartz and PTFE can take longer depending on availability — ask over WhatsApp before you commit to a date with your own customer.
What else is this kind of heater called?
It also goes by immersion heater, tank heater, submersible heater and chemical bath heater. It is the heater that goes down into the solution in your plating or process tank.
Could it contaminate my bath?
Yes, and it is the risk fewest people see coming. A sheath that corrodes releases its own metal into the solution, and that shows up in the finish on your parts before the heater ever perforates. That is the argument for paying for titanium or quartz where they belong: it is not about the life of the heater, it is about the production run.
Does it come with low-level protection?
It is strongly recommended and we build it in. A level control that cuts the heater before it is left exposed prevents the most common and most dangerous failure in a process tank. We can assemble it together with the control panel if you need that.
I don't have a drawing. How do I get a quote?
Send us a photo of your tank and of the heater you are replacing, and tell us what solution you are heating, at what concentration, at what temperature, and how many liters the tank holds. With that we settle the material, the wattage, the shape and the mounting, horizontal or vertical on the tank wall.
CATÁLOGO · MÁS MODELOS

¿Buscas otro material o configuración?

Browse all available models for plating and chemical bath heaters.
Explorar catálogo